Cracks in castings are a common problem in the casting manufacturing process. The causes are complex and varied, mainly including internal defects in castings, temperature stress, pressure stress, unreasonable casting design, and improper cooling measures.
I. Causes of casting cracks
1. Internal defects in castings:
Internal defects such as pores, slag inclusions, and inclusions may cause stress concentration, thereby causing cracks.
2. Temperature stress:
Castings will go through cooling and solidification stages during the casting process. If the cooling rate is uneven or the temperature changes too quickly, temperature stress will be generated inside the casting, which may cause cracks.
3. Pressure stress:
Castings may be subject to external pressure during the casting process, such as stress during pouring, cooling, or processing. When these stresses exceed the bearing capacity of the casting material, cracks may occur.
4. Unreasonable casting design:
The design of the casting may have an unreasonable structure or uneven wall thickness, which may lead to stress concentration and thus cause cracks.
5. Improper cooling measures:
Unreasonable cooling speed and method may lead to uneven temperature distribution inside the casting, which in turn causes cracks.
II. Methods to prevent casting cracks
1. Improve the structure of the casting:
The wall thickness should be uniform, and transition fillets should be made at the corners to reduce stress concentration. For wheel castings, the spokes can be made into a curved shape to disperse stress when necessary.
2. Improve the smelting quality of alloy materials:
Use refining and degassing processes to remove oxide inclusions and gases in the molten metal and control the content of harmful impurities.
3. Use correct casting process measures:
Make the casting solidify simultaneously to reduce the tendency of hot cracks and cold cracks. Reasonably set the position and size of the pouring and riser to make the cooling rate of each part of the casting as uniform as possible. Extend the residence time of the casting in the sand mold to further uniformize the temperature of the thicker and thinner parts of the casting, and reduce the temperature difference and thermal stress.
4. Increase the yield of the sand mold and sand core:
After the casting solidifies, remove the box press iron as soon as possible, loosen the sandbox fastening device, etc., to reduce the shrinkage resistance of the casting and promote uniform cooling of all parts of the casting.
5. Aging heat treatment:
Castings with large casting stress should be subjected to aging heat treatment in time to eliminate excessive residual stress and avoid cold cracks.
6. Control the unpacking time and cooling speed:
Avoid unpacking too early to avoid large internal stress in the casting and cracks. Control the cooling speed to avoid temperature stress concentration caused by too fast or too slow cooling.
7. Use appropriate pre-heat treatment:
Such as spheroidizing annealing or aging treatment to eliminate the internal stress of castings and forgings in time.